What it is made of
Iron with about 16–18 % chromium, 10–14 % nickel and 2–3 % molybdenum, and at most 0.03 % carbon (the "L" is for low carbon). Chromium makes it stainless; molybdenum adds resistance to salt.
316L is the "marine grade" stainless steel of boat fittings, surgical tools and food equipment. Printed by laser powder-bed fusion it comes out fully solid and, for most uses, stronger than the same steel bought as bar.
Values for laser powder-bed 316L as printed (not heat-treated), from published studies and powder makers' data sheets, beside ordinary annealed 316L bar. We do not test every part; treat them as a guide.
| Property | Printed 316L | 316L bar, annealed | What it means |
|---|---|---|---|
| Tensile strength | about 600–700 MPa | about 485–620 MPa | How hard you can pull before it breaks. |
| Yield strength | about 450–550 MPa | about 170–310 MPa | How hard you can pull before it bends for good. Printing's very fine grain makes it much higher. |
| Elongation at break | about 30–45 % | about 40–60 % | How far it stretches before breaking: a little less, still very tough. |
| Density | about 99.8 % of solid | 100 % | 7.98 g/cm³ for printed parts in our calculator. |
| Hardness | about 200–230 HV | about 150–200 HV | Scratches less easily than bar. |
Iron with about 16–18 % chromium, 10–14 % nickel and 2–3 % molybdenum, and at most 0.03 % carbon (the "L" is for low carbon). Chromium makes it stainless; molybdenum adds resistance to salt.
It resists fresh water, sweat, most foods and sea air. Like any stainless steel it can stain in strong chlorides (pool water, bleach) left on for long. Rinse and dry; the grainy printed surface holds dirt more than polished steel.
Essentially not. 316L is austenitic, which is non-magnetic. A strong magnet may feel a very faint pull on some printed parts, never enough to hold on.
316L is a food-grade and body-jewelry alloy. A printed surface, though, has microscopic pores and grain that are harder to clean than polished steel, so we do not certify parts for food contact or implants.
It keeps its strength well beyond any kitchen or engine-bay temperature. Heated in air from about 300 to 600 °C it takes on temper colors: straw, gold, bronze, purple, blue. That is a way to color parts.
It drills, taps, files and polishes like ordinary stainless steel. Use sharp tools and slow speeds; it work-hardens if a tool rubs instead of cutting.